TEGO In Action

Before Transition

After Transition

* Pre-Transition appears darker than actual due to being mounted on a solid white surface for testing.

**Transition time from before to after less than 30 seconds

TEGO Specifications

Before Transition

Total Solar Energy Transmitted
Total Solar Energy Transmitted 42%
Total Solar Energy Rejected
Total Solar Energy Rejected 50%
Total Solar Energy Reflected
Total Solar Energy Reflected 25%
Total Solar Energy Absorbed
Total Solar Energy Absorbed 33%
Visible Light Transmitted
Visible Light Transmitted 72%
Visible Light Reflected Exterior
Visible Light Reflected Exterior 12%
Visible Light Reflected Interior
Visible Light Reflected Interior 9%
Infrared Rejection
Infrared Rejection 79%
UV Rejection
UV Rejection 99.8%
Visible Light Glare Reduction
Visible Light Glare Reduction 30%
Solar Heat Gain Coefficient
Solar Heat Gain Coefficient 0.49
Shading Coefficient
Shading Coefficient 0.54
Coefficient of Conductivity
Coefficient of Conductivity 0.20
Radiance
Radiance 0.84
"U" Factor
"U" Factor 1.06

After Transition

Total Solar Energy Transmitted
Total Solar Energy Transmitted 37%
Total Solar Energy Rejected
Total Solar Energy Rejected 55%
Total Solar Energy Reflected
Total Solar Energy Reflected 27%
Total Solar Energy Absorbed
Total Solar Energy Absorbed 36%
Visible Light Transmitted
Visible Light Transmitted 55%
Visible Light Reflected Exterior
Visible Light Reflected Exterior 13%
Visible Light Reflected Interior
Visible Light Reflected Interior 11%
Infrared Rejection
Infrared Rejection 82%
UV Rejection
UV Rejection 99.8%
Visible Light Glare Reduction
Visible Light Glare Reduction 46%
Solar Heat Gain Coefficient
Solar Heat Gain Coefficient 0.44
Shading Coefficient
Shading Coefficient 0.50
Coefficient of Conductivity
Coefficient of Conductivity 0.20
Radiance
Radiance 0.84
"U" Factor
"U" Factor 1.06